Perbandingan antarane 12 titik tutup meneng lan hex bolt: Ing tembung prasaja, tutup meneng minangka "versi meningkat" khusus dirancang kanggo syarat kinerja dhuwur tartamtu. Kaluwihan inti dumunung ing papan instalasi sing luwih cilik, kapasitas torsi sing luwih dhuwur, lan kinerja anti-loosening sing luwih kuat, nanging uga mbutuhake alat lan anggaran sing luwih dhuwur. Tabel ing ngisor iki bakal mbantu sampeyan luwih ngerti beda antarane rong jinis sekrup.
| Proyek | 12 titik tutup meneng | Hex bolt |
| Desain sirah | Nyedhiyakake 12 titik kontak | Hexagon standar nyedhiyakake 6 titik kontak. |
| ruang operasi | Rotasi mung mbutuhake 30 °. | Rotasi mbutuhake 60 °. |
| Persyaratan Alat | Soket 12-titik khusus utawa kunci lintang kudu digunakake. | Alat kasebut nduweni versatility sing dhuwur banget lan bisa ditrapake kanggo meh kabeh kunci pas lan soket. |
| Transmisi torsi | Banget | Rata-rata |
| Kinerja anti-loosening | Dilengkapi flange serrated, nambah gesekan | Biasane digunakake bebarengan karo spring washers |
| Tekanan lumahing | Ngisor | Luwih dhuwur |
| Kinerja benang anti-slip | Banget | Rata-rata |
| Efisiensi instalasi | Kacepetan instalasi kira-kira 60% luwih cepet tinimbang bolt heksagonal. | Standar lan universal |
| biaya | Luwih dhuwur | Ngisor |
| Skenario sing ditrapake Lingkungan sing atos | mesin automotive, aerospace, Petrokimia, heavy machinery, etc lapangan Widely Applied | mesin umum, struktur bangunan, pangopènan saben dina, lsp. |
(1)Standar apa sing cocog karo sekrup tutup 12 titik sampeyan?
A: Kita nggawe kanthi ketat miturut DIN 34800 (standar Jerman), ASME B18.2.5M (standar metrik Amerika) lan IFI 115 (bolt gear bevel rolas-titik bevel Amerika).
(2) Bahan apa sing sampeyan tawarake?
A: We offer bahan ing ngisor iki lan gelar kinerja:
Baja karbon, baja paduan, baja tahan karat, bahan khusus: paduan Titanium, paduan suhu dhuwur (kayata Inconel 718), paduan aluminium, lsp.
(3) Opsi perawatan permukaan apa sing kasedhiya kanggo sekrup tutup 12 titik? Carane tahan kanggo semprotan uyah?
| Mon | M22 | M24 | M27 | M30 | M33 | M36 | M39 | M42 | M45 | M48 | M52 |
| P | 2.5 | 3 | 3 | 3.5 | 3.5 | 4 | 4 | 4.5 | 4.5 | 5 | 5 |
| dc maks | 33.3 | 38.1 | 38.1 | 42.8 | 47.5 | 52.3 | 57 | 61.7 | 66.5 | 76 | 76 |
| dc min | 32.68 | 37.48 | 37.48 | 42.18 | 46.88 | 51.56 | 56.26 | 60.96 | 65.76 | 75.26 | 75.26 |
| ds maks | 22 | 24 | 27 | 30 | 33.0 | 36 | 39 | 42.0 | 45.0 | 48 | 52 |
| ds min | 21.79 | 23.79 | 26.79 | 29.79 | 32.75 | 35.75 | 38.75 | 41.75 | 44.75 | 47.75 | 51.7 |
| e min | 25.4 | 27.7 | 27.7 | 34.6 | 36.90 | 41.60 | 47.30 | 47.30 | 53.10 | 57.70 | 57.70 |
| h maks | 6.9 | 7.98 | 7.98 | 9.21 | 9.62 | 10.82 | 12.71 | 12.56 | 15.65 | 16.1 | 16.1 |
| h min | 6.54 | 7.35 | 7.35 | 8.78 | 9.19 | 10.39 | 12.28 | 12.13 | 15.13 | 15.58 | 15.58 |
| k maks | 22.36 | 25.56 | 25.56 | 28.96 | 32.0 | 35.2 | 38.3 | 41.4 | 44.7 | 51.03 | 51.03 |
| k min | 22.04 | 25.24 | 25.24 | 28.54 | 31.6 | 34.80 | 37.90 | 41.00 | 44.30 | 50.57 | 50.57 |
| r maks | 1 | 1.2 | 1.20 | 1.4 | 1.60 | 1.60 | 1.80 | 1.80 | 2.00 | 2.20 | 2.20 |
| r min | 0.75 | 0.95 | 0.95 | 1.15 | 1.35 | 1.35 | 1.55 | 1.55 | 1.75 | 1.82 | 1.82 |
| s maks | 22 | 24 | 24 | 30 | 32.00 | 36.00 | 41.00 | 41.00 | 46.0 | 50.0 | 50.0 |
| s min | 21.79 | 23.79 | 23.79 | 29.79 | 31.75 | 35.75 | 40.75 | 40.75 | 45.75 | 49.75 | 49.75 |
Electro-galvanizing: Seng biru-putih / Kuning, tahan kanggo semprotan uyah kanggo 48 - 120 jam
Paduan seng-nikel: Perak-abu-abu/ireng, tahan kabut uyah sajrone 500 - 1000 jam
Dakro/Geomet: Abu-abu salaka matte, tahan semprotan uyah luwih saka 1000 jam
Hot-dip galvanizing: Lapisan tebal abu-abu perak, tahan kanggo semprotan uyah kanggo 500 - 1000 jam
Nguripake ireng: Mung 12-24 jam
(4)Apa alat khusus sing dibutuhake sajrone instalasi?
A: Soket 12-titik utawa kunci kothak 12-titik dibutuhake.
(5)Apa produk sampeyan bisa digunakake maneh?
Bisa digunakake maneh yen wis dipriksa kanthi ketat sadurunge saben nggunakake kanggo mesthekake yen ora ana kerusakan (ora nyandhang ing sirah rolas titik, ora ana goresan ing benang, lan ora ana deformasi ing permukaan flange). Nanging, kanggo produk 12.9 kelas dhuwur-kekuatan, disaranake ora ngluwihi 3 panggunaan.