Yen sampeyan butuh perlindungan karat paling apik utawa kacang-kacangan non-magnetik, efisiensi kacepetan weld hexagon kanthi flang teka ing stainless stainless austenitik kaya aisi 304 utawa 316 / l. Jinis-jinis kasebut bisa uga nglawan karat, bahan kimia, lan panas. Sing baja stainless bisa mlaku ing papan kaya pangolahan panganan, farmasi, setelan marine, lan lingkungan kimia sing bener-bener.
Mon | M5 | M6 | M8 | M10 | M12 | M14 | M16 |
P | 0.8 | 1 | 1.25 | 1.5 | 1.75 | 2 | 2 |
H1 Max | 0.9 | 0.9 | 1.1 | 1.3 | 1.3 | 1.3 | 1.3 |
H1 min | 0.7 | 0.7 | 0.9 | 1.1 | 1.1 | 1.1 | 1.1 |
DC Max | 15.5 | 18.5 | 22.5 | 26.5 | 30.5 | 33.5 | 36.5 |
DC Min | 14.5 | 17.5 | 21.5 | 25.5 | 29.5 | 32.5 | 35.5 |
E min | 8.2 | 10.6 | 13.6 | 16.9 | 19.4 | 22.4 | 25 |
H max | 1.95 | 2.25 | 2.75 | 3.25 | 3.25 | 4.25 | 4.25 |
H min | 1.45 | 1.75 | 2.25 | 2.75 | 2.75 | 3.75 | 3.75 |
b max | 4.1 | 5.1 | 6.1 | 7.1 | 8.1 | 8.1 | 8.1 |
B min | 3.9 | 4.9 | 5.9 | 6.9 | 7.9 | 7.9 | 7.9 |
K Min | 4.7 | 6.64 | 9.64 | 12.57 | 14.57 | 16.16 | 18.66 |
k max | 5 | 7 | 10 | 13 | 15 | 17 | 19.5 |
s max | 8 | 10 | 13 | 16 | 18 | 21 | 24 |
s min | 7.64 | 9.64 | 12.57 | 15.57 | 17.57 | 20.16 | 23.16 |
Kauntungan:
Efisiensi Dhuwur Hexagon Kacang Hexagon kanthi flange nindakake sawetara perkara sing penting. Kerjane kaya mesin cuci sing dibangun, nyebarake beban lan tetep permukaan alus saka rusak. Iki uga menehi wilayah sing luwih gedhe, studier kanggo nggarap nalika welding. Sing paling penting, flange mbantu dheweke tetep luwih apik tinimbang kacang hem biasa, sanajan ana geter, kejut, utawa beban sing bisa ditindakake.
Kinerja anti-korosi sing apik banget:
Cara umum kanggo nambani efisiensi High Hexagon karo flange yaiku flange yaiku plating zink, biru, biru, galvine panas banget kanggo lingkungan sing angel, lan lapisan dacromet. Sing baja stainless steel (A2 / A4) ora butuh lapisan ekstra; Dheweke nolak karat dhewe.